產(chǎn)品詳情
物理性能 | 值/單位 | 測(cè)試標(biāo)準(zhǔn) | 測(cè)試條件 |
---|---|---|---|
密度 |
1.2 g/cm3 | ISO 1183 |
|
比重 |
1.19 - | ASTM D792 |
|
熔體體積流動(dòng)速率(MVR) |
|||
260°C/2.16 kg |
15 cm3/10 min | ISO 1133 |
|
熔體質(zhì)量流動(dòng)速率(MFR) |
|||
260°C/2.16 kg |
16 g/10min | ASTM D1238 |
|
收縮率 |
|||
縱向(Flow) |
0.4~0.6 % | Internal |
flow, 3.2 mm |
吸水率 |
0.2 % | ISO 62 |
23°C/sat |
吸濕率 |
0.1 % | ISO 62 |
23°C / 50% RH |
機(jī)械性能 | 值/單位 | 測(cè)試標(biāo)準(zhǔn) | 測(cè)試條件 |
拉伸強(qiáng)度 |
|||
屈服(yld) |
65 Mpa | ASTM D638 |
Type I, 50 mm/min |
屈服(yld) |
65 Mpa | ISO 527 |
50 mm/min |
斷裂(brk) |
50 Mpa | ISO 527 |
50 mm/min |
斷裂(brk) |
58 Mpa | ASTM D638 |
Type I, 50 mm/min |
拉伸延伸率 |
|||
屈服(yld) |
4.1 % | ASTM D638 |
Type I, 50 mm/min |
屈服(yld) |
4 % | ISO 527 |
50 mm/min |
斷裂(brk) |
100 % | ASTM D638 |
Type I, 50 mm/min |
斷裂(brk) |
90 % | ISO 527 |
50 mm/min |
彎曲強(qiáng)度 |
|||
屈服(yld) |
104 Mpa | ASTM D790 |
1.3 mm/min, 50 mm span |
屈服(yld) |
96 Mpa | ISO 178 |
2 mm/min |
彎曲模量 |
2750 Mpa | ASTM D790 |
1.3 mm/min, 50 mm span |
彎曲模量 |
2500 Mpa | ISO 178 |
2 mm/min |
拉伸模量 |
2950 Mpa | ASTM D638 |
50 mm/min |
拉伸模量 |
2530 Mpa | ISO 527 |
1 mm/min |
沖擊性能 | 值/單位 | 測(cè)試標(biāo)準(zhǔn) | 測(cè)試條件 |
簡(jiǎn)支梁缺口(Charpy Notched) |
|||
-30℃ (-22℉) |
10 kJ/m2 | ISO 179/1eA |
V-notch Edgew 80*10*3 sp=62mm |
23℃ (73℉) |
20 kJ/m2 | ISO 179/1eA |
V-notch Edgew 80*10*3 sp=62mm |
懸臂梁缺口(Izod Notched) |
|||
-30℃ (-22℉) |
100 J/m | ASTM D256 |
|
-30℃ (-22℉) |
10 kJ/m2 | ISO 180/1A |
80*10*3 |
23℃ (73℉) |
500 J/m | ASTM D256 |
|
23℃ (73℉) |
20 kJ/m2 | ISO 180/1A |
80*10*3 |
儀器化落鏢沖擊能量 |
|||
23℃ (73℉)總能量 |
65 J | ASTM D3763 |
|
熱學(xué)性能 | 值/單位 | 測(cè)試標(biāo)準(zhǔn) | 測(cè)試條件 |
熱變形溫度(HDT) |
|||
0.45 Mpa (66 psi)(4.6kg/cm2) |
100 °C | ASTM D648 |
3.2mm, unannealed |
1.8 Mpa (264 psi)(18.6kg/cm2) |
89 °C | ASTM D648 |
3.2mm, unannealed |
1.8 Mpa (264 psi)(18.6kg/cm2) |
99 °C | ASTM D648 |
6.4 mm, unannealed |
1.8 Mpa (264 psi)(18.6kg/cm2) |
93 °C | ISO 75/Af |
Flatw 80*10*4 sp=64mm |
維卡軟化溫度(Vicat) |
106 °C | ASTM D1525 |
Rate B/50 |
維卡軟化溫度(Vicat) |
113 °C | ISO 306 |
Rate B/120 |
維卡軟化溫度(Vicat) |
110 °C | ISO 306 |
Rate B/50 |
相對(duì)溫度指數(shù)(RTI) |
|||
沖擊w/impact,- |
90 °C | UL 746B |
|
電氣Elec,- |
90 °C | UL 746B |
|
強(qiáng)度w/o impact,- |
90 °C | UL 746B |
|
線性膨脹系數(shù)(CLTE) |
|||
縱向(Flow) |
62.5 E-6/°C | ASTM E831 |
-40°C to 40°C, flow |
縱向(Flow) |
62 E-6/°C | ISO 11359-2 |
-40°C to 40°C, flow |
橫向(Across Flow) |
53.5 E-6/°C | ASTM E831 |
-40°C to 40°C, xflow |
橫向(Across Flow) |
54 E-6/°C | ISO 11359-2 |
-40°C to 40°C, xflow |
球壓痕溫度 |
75 °C | IEC 60695-10-2 |
PASS |
燃燒性能 | 值/單位 | 測(cè)試標(biāo)準(zhǔn) | 測(cè)試條件 |
UL 防火等級(jí) |
|||
V-2 |
0.4 mm | UL94 |
|
V-1 |
0.6 mm | UL94 |
|
V-0 |
0.75 mm | UL94 |
|
5VB |
1.5 mm | UL94 |
|
5VA |
3 mm | UL94 |
|
灼熱絲可燃性指數(shù)(GWFI) |
|||
0.75mm |
960 °C | IEC 60695-2-12 |
pass |
灼熱絲點(diǎn)燃溫度(GWIT) |
|||
1.0mm |
825 °C | IEC 60695-2-13 |
|
3.0mm |
800 °C | IEC 60695-2-13 |
|
電學(xué)性能 | 值/單位 | 測(cè)試標(biāo)準(zhǔn) | 測(cè)試條件 |
相比漏電起痕指數(shù)(CTI ) |
|||
- |
3 PLC | UL 746A |
|
熱線圈起燃性(HWI) |
3 PLC | UL 746A |
|
高電流弧起燃性(HAI) |
0 PLC | UL 746A |